We have a very strict control
system according to the America Four Point
Standard. The total score can be limited
within 24 /100 square yards.(AATCC standard)
Item
Method
Standard
(1)Crocking
AATCC8
Dry
above 4 Grade
Wet
above 3 Grade
(2)Tastness to light
AATCC16E
(10 depigment unit)
above
4 Grade
(3)fastness to washing
AATCC61
above class-4
(4)fastness to perspiration
AATCC 15
color-changing:class-4
staining:class-3
(5)After-washing size
AATCC135
Exterior stability
Normal fabric
-3%
elastic fabric
(Lycra more than 2 percent)
-5%no
more length
(6)Tensile strength
ASTM D5034
≥25Lbs
(7)Tear strength
ASTM D1424
≥1.5Lbs
(8)Seam slippage
ASTM D1683
≥15Lbs
(9)formaldehyde
AATCC 112
≤75PPm Recovery
(10)Stretch and Recovry
Recory
ASTM
D3107
Ratio 96%
Stretch at least 15-20%
(11)PH
AATCC
81
5.5-8.5
(12)Pilling
ASTM
D3512
above class-3
(13)Grind-pro ofand pilling
ASTM
D4966
above class-3.5